# Commission Implementing Decision (EU) 2016/1032 of 13 June 2016 establishing best available techniques (BAT) conclusions, under Directive 2010/75/EU of the European Parliament and of the Council, for the non-ferrous metals industries (notified under document C(2016) 3563) (Text with EEA relevance), Division BAT 96

Extent: E+W+S+N.I.

In order to reduce dust and metal emissions to air (other than those that are routed to the sulphuric acid or liquid SO2 plant) from charging, smelting and tapping in primary and secondary lead and/or tin production, BAT is to use a bag filter.
BAT-associated emission levels: See Table 24.
Table 24
BAT-associated emission levels for dust and lead emissions to air (other than those that are routed to the sulphuric acid or liquid SO2 plant) from charging, smelting and tapping in primary and secondary lead and/or tin production
As a daily average or as an average over the sampling period.
Dust emissions are expected to be towards the lower end of the range when emissions are above the following levels: 1 mg/Nm3 for copper, 0,05 mg/Nm3 for arsenic, 0,05 mg/Nm3 for cadmium.
As an average over the sampling period.
Parameter
BAT-AEL (mg/Nm3)
Dust
2-4
Pb
≤ 1

---
Source: https://www.legislation.gov.uk/eudn/2016/1032/annex/division/1.4/division/1.4.1/division/1.4.1.2/division/bat+96 (the official version)