Non-alloy aluminium shall have an aluminium content of at least 99,5 % and the alloys referred to in point (b) of Article 1(1) shall display adequate resistance to intercrystalline corrosion at maximum working temperature.
Moreover, these materials shall satisfy the following requirements:
(a) they shall be supplied in an annealed state;
(b) they shall have the following mechanical characteristics per product:
the maximum tensile strength Rm,max shall be no more than 350 N/mm2,
the elongation after fracture shall be:
A ≥ 16 % if the test piece is taken parallel to the direction of rolling,
A ≥ 14 % if the test piece is taken perpendicular to the direction of rolling.

---
Source: https://www.legislation.gov.uk/eudr/2014/29/annex/I/division/1/division/1.1/division/1.1.2 (the official version)
Page: https://openlegislation.uk/eu-directive-2014-29/annex-I/division-1/division-1.1/division-1.1.2
Contains public sector information licensed under the Open Government Licence v3.0. Source: legislation.gov.uk, The National Archives.