OpenLegislation

Division 1.6.1.1 Combustible substance

United Kingdom

Original text. Later amendments are not shown.

Dried, fibrous cellulose with a fibre length between 50 and 250 µm and a mean diameter of 25 µm,f1 is used as the combustible material. It is dried to constant weight in a layer not more than 25 mm thick at 105 oC for 4 hours and kept in a desiccator, with desiccant, until cool and required for use. The water content of the dried cellulose should be less than 0.5% by dry massf2. If necessary, the drying time should be prolonged to achieve this.f3 The same batch of cellulose is to be used throughout the test.

Annotations

Footnotes

f1

e.g. Whatman Column Chromatographic Cellulose Powder CF 11, catalogue no 4021 050

f2

Confirmed by (e.g.) Karl-Fisher titration

f3

Alternatively, this water content can also be achieved by (e.g.) heating at 105 oC under vacuum for 24 h